Differences
This shows you the differences between two versions of the page.
| Both sides previous revision Previous revision Next revision | Previous revision | ||
| mini_flow [2018/12/27 22:35] – [setup] yair | mini_flow [2018/12/31 12:45] (current) – [test setup] yair | ||
|---|---|---|---|
| Line 5: | Line 5: | ||
| we are intrested in small reflow ovens for workshops, to remove the need for soldering smd with cheap irons. | we are intrested in small reflow ovens for workshops, to remove the need for soldering smd with cheap irons. | ||
| - | ==== setup ==== | + | mybe call it uBake ? | 
| + | ==== test setup ==== | ||
| + | |||
| + | {{: | ||
| first tested on bench with no heat load.\\ | first tested on bench with no heat load.\\ | ||
| Line 13: | Line 16: | ||
| using a benchtop psu or lm317(?) you can make a very simple reflow profile.\\ | using a benchtop psu or lm317(?) you can make a very simple reflow profile.\\ | ||
| - | {{ ::basic.mp4 |}} | + | {{:: | 
| placed the ceramic heater on top of a huge copper heatsink (idiot) | placed the ceramic heater on top of a huge copper heatsink (idiot) | ||
| + | |||
| + | |||
| {{: | {{: | ||
| - | then moved to a more suitable setup and it was a breeze | + | then moved to a more suitable setup | 
| - | {{: | + | {{: | 
| - | {{:ubake.png?500}} | + | i used microprint 2004p (Sn62 Pb36 Ag2, 20-38 µm (T4)) ({{ :: | 
| + | with a claimed melting point of 179°C | ||
| - | a quickiFX(?) low temp solder didn't zip into place\\ | + | {{:: | 
| - | i was shocked by the low temp i couldn' | + | |
| {{: | {{: | ||
| Line 38: | Line 43: | ||
| {{: | {{: | ||
| - | {{: | ||
| Line 46: | Line 50: | ||
| {{: | {{: | ||
| + | ==== PID ==== | ||
| + | https:// | ||
| + | and polyfuse? | ||